| Chemical Composition (XRF Verified) |
16–18% Cr, 10–14% Ni, 2.0–3.0% Mo |
18.0–20.0% Cr, 8.0–10.5% Ni, <0.08% C |
16.0–18.0% Cr, <0.75% Ni (Ferritic Magnetic) |
13–15% Cr, 0.8–1.5% Ni, 5.5–7.5% Mn |
| ASTM B117 5% NaCl Salt-Spray Endurance |
240+ Hours (Zero Pitting in Acidic Sauces) |
96+ Hours (Zero Red Rust / Passivated Ra ≤ 0.25μm) |
48 Hours (Used for Outer Induction Capsule Base) |
12–24 Hours (Prone to Intergranular Rust) |
| LFGB / FDA / EU 1935/2004 Heavy Metal Migration |
100% Pass (Pb, Cd, Cr VI, Ni migration < 0.01 mg/kg) |
100% Pass (Certified for Boiling Acidic Food Contact) |
100% Pass (Outer Magnetic Base & Dry Utensils) |
Risk of Manganese Migration in 4% Acetic Acid |
| Magnetic Permeability (Induction Cooktop) |
Non-Magnetic (Requires SUS430 Bonded Outer Layer) |
Non-Magnetic (Bonded with Aluminum + SUS430 Base) |
Highly Ferromagnetic (μr > 600 · Instant Eddy Heating) |
Weakly Magnetic After Cold Work Hardening |
| Recommended Nice Kitchen Product Line |
Luxury Flagship Stock Pots & Coastal Hotel Chafers |
Core Cookware Interiors, Chafing Food Pans, Bento & Bowls |
Outer Capsule Induction Discs on All Cookware & Kettles |
Budget Non-Acidic Dry Storage & Utility Basins Only |